POM N2320-003 德國巴斯夫公司 物性數(shù)據(jù) |
①原料描述部分 |
|||||||
暫無此原料描述部分┄ |
|||||||
②原料技術(shù)數(shù)據(jù) |
|||||||
性能項(xiàng)目 |
試驗(yàn)條件[狀態(tài)] |
測試方法 |
測試數(shù)據(jù) |
數(shù)據(jù)單位 |
|||
基本性能 |
熔融指數(shù) |
220℃/10kg |
--- |
7.5 |
cm3/10min |
||
吸水率 |
--- |
--- |
0.8 |
% |
|||
吸濕率 |
--- |
--- |
0.2 |
% |
|||
密度 |
--- |
--- |
1400 |
Kg/cm3 |
|||
物理性能 |
??s率 |
水平方向 |
--- |
2.09 |
% |
||
機(jī)械性能 |
拉伸模量 |
--- |
--- |
2700 |
MPa |
||
拉伸屈服強(qiáng)度 |
--- |
--- |
65 |
MPa |
|||
屈服伸長率 |
--- |
--- |
9.4 |
% |
|||
斷裂伸長率 |
--- |
--- |
27 |
% |
|||
拉伸模量 |
1h |
--- |
1800 |
MPa |
|||
Charpy沖擊強(qiáng)度 |
23℃ |
--- |
210 |
KJ/m |
|||
Charpy缺口沖擊強(qiáng)度 |
23℃ |
--- |
6 |
KJ/m |
|||
電氣性能 |
介電常數(shù) |
100HZ |
--- |
3.8 |
--- |
||
體積電阻率 |
--- |
--- |
1E13 |
Ohm |
|||
表面電阻率 |
--- |
--- |
1E13 |
Ohm |
|||
介電強(qiáng)度 |
--- |
--- |
40 |
Kv/mm |
|||
熱 性 能 |
線膨脹系數(shù) |
水平方向 |
--- |
1.1 |
E-4/℃ |
||
燃燒率 |
1.6mm |
--- |
HB |
Class |
|||
熔點(diǎn) |
10℃/min |
--- |
167 |
℃ |
|||
熱變形溫度 |
1.80MPa |
--- |
105 |
℃ |
|||
維卡軟化溫度 |
50℃/h50n |
--- |
150 |
℃ |
|||
其它性能 |
氧指數(shù) |
--- |
--- |
15 |
% |
||
損耗角 |
100HZ |
--- |
10 |
E-4 |